ATI Allvac® Nickelvac® 901 Nickel Superalloy, Heat Treatment: 1010°C (1850°F) + Age
Seller in Houston price: $2083 per MT
Seller in Lima price: $2270 per MT
Seller in Singapore price: $2510 per MT
ATI Allvac® Nickelvac® 901 Nickel Superalloy, Heat Treatment: 1010°C (1850°F) + Age in Nickel Alloy, Superalloy
FOLLOW US ON
3 prices for ATI Allvac® Nickelvac® 901 Nickel Superalloy, Heat Treatment: 1010°C (1850°F) + Age
Seller from Houston – 2021-06-30:
Seller from Houston work with company: Solvay, Teknor Apex Company, SABIC Innovative Plastics (GE Plastics), ALIMEX GmbH
Price: $2083 per MT
Seller from Lima – 2021-06-16:
Seller from Lima work with company: 3M, Solvay, SABIC Innovative Plastics (GE Plastics), ALIMEX GmbH
Price: $2270 per MT
Seller from Singapore – 2021-06-18:
Seller from Singapore work with company: 3M, Solvay, SABIC Innovative Plastics (GE Plastics), ALIMEX GmbH
Price: $2510 per MT