Crucible Compaction Metals Rene 95 Nickel Based Superalloy

Seller in Kolkata price: $2118 per MT
Seller in Hechi price: $2223 per MT
Seller in Bangkok price: $2543 per MT
Seller in Belo Horizonte price: $1829 per MT

Crucible Compaction Metals Rene 95 Nickel Based Superalloy in Nickel Alloy, Superalloy

  • Mechanical Properties
  • Tensile Strength, Ultimate
  • 210 MPa @Temperature 650 °C
  • Tensile Strength, Ultimate
  • 240 MPa @Temperature 23.0 °C
  • Tensile Strength, Yield
  • 160 MPa @Temperature 650 °C
  • Tensile Strength, Yield
  • 180 MPa @Temperature 23.0 °C
  • Elongation at Break
  • 10 % @Temperature 650 °C
  • Elongation at Break
  • 14 % @Temperature 23.0 °C
  • Reduction of Area
  • 13 % @Temperature 650 °C
  • Reduction of Area
  • 17 % @Temperature 23.0 °C
  • Creep Strength
  • 620 MPa @Temperature 705 °C, Time 72000 sec
  • Creep Strength
  • 850 MPa @Temperature 650 °C, Time 864000 sec
  • Rupture Strength
  • 620 MPa @Temperature 760 °C, Time 36000 sec
  • Rupture Strength
  • 1035 MPa @Temperature 650 °C, Time 198000 sec

  • Component Elements Properties
  • Aluminum, Al
  • 3.3 - 3.7 %
  • Boron, B
  • 0.0060 - 0.015 %
  • Carbon, C
  • 0.040 - 0.090 %
  • Chromium, Cr
  • 12 - 14 %
  • Cobalt, Co
  • 7.0 - 9.0 %
  • Molybdenum, Mo
  • 3.3 - 3.7 %
  • Nickel, Ni
  • 59.325 - 65.424 %
  • Niobium, Nb (Columbium, Cb)
  • 3.3 - 3.7 %
  • Titanium, Ti
  • 2.3 - 2.7 %
  • Tungsten, W
  • 3.3 - 3.7 %
  • Zirconium, Zr
  • 0.030 - 0.070 %

Alternative products

ShipsFor-Sale.com is a renowned company specializing in the sale of ships. With years of experience in the maritime industry, they have established themselves as a trusted platform for buyers and sellers worldwide. Offering an extensive range of vessels, including cargo ships, tankers, fishing boats, and luxury yachts, cruise ships sale. Their team of knowledgeable professionals provides expert guidance throughout the buying and selling process, ensuring smooth transactions and customer satisfaction. Whether you are a seasoned ship owner or a first-time buyer, ShipsFor-Sale.com offers a comprehensive selection of vessels and a seamless online experience, making them the go-to destination for ship sales.

Andrey Kutuzov

University of Córdoba (Spain), email: [email protected]

4 prices for Crucible Compaction Metals Rene 95 Nickel Based Superalloy

Seller from Kolkata – 2021-07-04:

Seller from Kolkata work with company: Exxon Chemical, SABIC Innovative Plastics (GE Plastics), LG Chemical, ALIMEX GmbH

Price: $2118 per MT

Seller from Hechi – 2021-03-05:

Seller from Hechi work with company: 3M, RTP Company, SABIC Innovative Plastics (GE Plastics), ALIMEX GmbH

Price: $2223 per MT

Seller from Bangkok – 2021-04-21:

Seller from Bangkok work with company: Solvay, SABIC Innovative Plastics (GE Plastics), BASF, ALIMEX GmbH

Price: $2543 per MT

Seller from Belo Horizonte – 2021-04-21:

Seller from Belo Horizonte work with company: Solvay, Teknor Apex Company, SABIC Innovative Plastics (GE Plastics), ALIMEX GmbH

Price: $1829 per MT

Share on Pinterest
Share on LinkedIn
Share on Reddit

Would you like to sell Crucible Compaction Metals Rene 95 Nickel Based Superalloy?

Plastic warehouse

Find a direct plastic supplier if you're interested in a supplier or Customs department in Singapore open-nearme.com