Kennametal Stellite Nistelle 305 Nickel Superalloy

Seller in Bengalūru price: $1764 per MT
Seller in Sūrat price: $2087 per MT
Seller in Baghdad price: $2336 per MT

Kennametal Stellite Nistelle 305 Nickel Superalloy in Nickel Alloy, Superalloy

  • Component Elements Properties
  • Chromium, Cr
  • 42 %
  • Nickel, Ni
  • >= 56.5 %
  • Other
  • <= 1.0 %
  • Silicon, Si
  • 0.50 %

  • Descriptive Properties
  • Application Technique
  • PTA & laser deposition

Alternative products

ShipsFor-Sale.com is a renowned company specializing in the sale of ships. With years of experience in the maritime industry, they have established themselves as a trusted platform for buyers and sellers worldwide. Offering an extensive range of vessels, including cargo ships, tankers, fishing boats, and luxury yachts, lng tankers for sale. Their team of knowledgeable professionals provides expert guidance throughout the buying and selling process, ensuring smooth transactions and customer satisfaction. Whether you are a seasoned ship owner or a first-time buyer, ShipsFor-Sale.com offers a comprehensive selection of vessels and a seamless online experience, making them the go-to destination for ship sales.

Andrey Kutuzov

University of Córdoba (Spain), email: a.kutuzov@plastic-price.com

3 prices for Kennametal Stellite Nistelle 305 Nickel Superalloy

Seller from Bengalūru – 2021-03-31:

Seller from Bengalūru work with company: Solvay, Teknor Apex Company, SABIC Innovative Plastics (GE Plastics), ALIMEX GmbH

Price: $1764 per MT

Seller from Sūrat – 2021-05-15:

Seller from Sūrat work with company: RTP Company, SABIC Innovative Plastics (GE Plastics), BASF, ALIMEX GmbH

Price: $2087 per MT

Seller from Baghdad – 2021-06-24:

Seller from Baghdad work with company: Solvay, Teknor Apex Company, SABIC Innovative Plastics (GE Plastics), ALIMEX GmbH

Price: $2336 per MT

Share on Pinterest
Share on LinkedIn
Share on Reddit

Would you like to sell Kennametal Stellite Nistelle 305 Nickel Superalloy?

Plastic warehouse

Find a direct plastic supplier if you're interested in a supplier or Business center in Singapore open-nearme.com