Kennametal Stellite Nistelle C4C Nickel Superalloy

Seller in Rio de Janeiro price: $2507 per MT
Seller in Phoenix price: $1718 per MT
Seller in Boston price: $2261 per MT
Seller in Saint Petersburg price: $2425 per MT

Kennametal Stellite Nistelle C4C Nickel Superalloy in Nickel Alloy, Superalloy

  • Component Elements Properties
  • Chromium, Cr
  • 16 %
  • Iron, Fe
  • <= 1.0 %
  • Molybdenum, Mo
  • 16 %
  • Nickel, Ni
  • >= 66 %
  • Silicon, Si
  • <= 1.0 %

  • Descriptive Properties
  • Application Technique
  • HVOF & thermal spray
  • Application Technique
  • PTA & laser deposition

Alternative products

ShipsFor-Sale.com is a renowned company specializing in the sale of ships. With years of experience in the maritime industry, they have established themselves as a trusted platform for buyers and sellers worldwide. Offering an extensive range of vessels, including cargo ships, tankers, fishing boats, and luxury yachts, chemical carrier for sale. Their team of knowledgeable professionals provides expert guidance throughout the buying and selling process, ensuring smooth transactions and customer satisfaction. Whether you are a seasoned ship owner or a first-time buyer, ShipsFor-Sale.com offers a comprehensive selection of vessels and a seamless online experience, making them the go-to destination for ship sales.

Andrey Kutuzov

University of Córdoba (Spain), email: [email protected]

4 prices for Kennametal Stellite Nistelle C4C Nickel Superalloy

Seller from Rio de Janeiro – 2021-05-08:

Seller from Rio de Janeiro work with company: 3M, Solvay, RTP Company, SABIC Innovative Plastics (GE Plastics)

Price: $2507 per MT

Seller from Phoenix – 2021-07-28:

Seller from Phoenix work with company: 3M, Solvay, SABIC Innovative Plastics (GE Plastics), ALIMEX GmbH

Price: $1718 per MT

Seller from Boston – 2021-05-31:

Seller from Boston work with company: 3M, Solvay, SABIC Innovative Plastics (GE Plastics), ALIMEX GmbH

Price: $2261 per MT

Seller from Saint Petersburg – 2021-07-02:

Seller from Saint Petersburg work with company: Solvay, RTP Company, SABIC Innovative Plastics (GE Plastics), ALIMEX GmbH

Price: $2425 per MT

Share on Pinterest
Share on LinkedIn
Share on Reddit

Would you like to sell Kennametal Stellite Nistelle C4C Nickel Superalloy?

Plastic warehouse

Find a direct plastic supplier if you're interested in a supplier or Homeowners' association in Singapore open-nearme.com