Kennametal Stellite Stellite® 6B solution heat-treated at 1232°C, 1.6 mm thick sheet

Seller in Ankara price: $1741 per MT

Kennametal Stellite Stellite® 6B solution heat-treated at 1232°C, 1.6 mm thick sheet in Cobalt Alloy, Superalloy

  • Physical Properties
  • Density
  • 8.387 g/cc

  • Mechanical Properties
  • Hardness, Brinell
  • 102 @Temperature 871 °C
  • Hardness, Brinell
  • 167 @Temperature 760 °C
  • Hardness, Brinell
  • 203 @Temperature 649 °C
  • Hardness, Brinell
  • 226 @Temperature 538 °C
  • Hardness, Knoop
  • 117 @Temperature 871 °C
  • Hardness, Knoop
  • 194 @Temperature 760 °C
  • Hardness, Knoop
  • 237 @Temperature 649 °C
  • Hardness, Knoop
  • 265 @Temperature 538 °C
  • Hardness, Rockwell A
  • 36 @Temperature 871 °C
  • Hardness, Rockwell A
  • 52 @Temperature 760 °C
  • Hardness, Rockwell A
  • 58 @Temperature 649 °C
  • Hardness, Rockwell A
  • 60 @Temperature 538 °C
  • Hardness, Rockwell B
  • 55 @Temperature 871 °C
  • Hardness, Rockwell B
  • 86 @Temperature 760 °C
  • Hardness, Rockwell B
  • 94 @Temperature 649 °C
  • Hardness, Rockwell B
  • 98 @Temperature 538 °C
  • Hardness, Vickers
  • 102 @Temperature 871 °C
  • Hardness, Vickers
  • 170 @Temperature 760 °C
  • Hardness, Vickers
  • 208 @Temperature 649 °C
  • Hardness, Vickers
  • 232 @Temperature 538 °C
  • Tensile Strength, Ultimate
  • 1007 MPa
  • Tensile Strength, Ultimate
  • 92.0 MPa @Temperature 1150 °C
  • Tensile Strength, Ultimate
  • 134 MPa @Temperature 1090 °C
  • Tensile Strength, Ultimate
  • 225 MPa @Temperature 982 °C
  • Tensile Strength, Ultimate
  • 385 MPa @Temperature 871 °C
  • Tensile Strength, Ultimate
  • 509 MPa @Temperature 816 °C
  • Tensile Strength, Yield
  • 632 MPa @Strain 0.200 %
  • Tensile Strength, Yield
  • 53.0 MPa @Strain 0.200 %, Temperature 1150 °C
  • Tensile Strength, Yield
  • 75.0 MPa @Strain 0.200 %, Temperature 1090 °C
  • Tensile Strength, Yield
  • 137 MPa @Strain 0.200 %, Temperature 982 °C
  • Tensile Strength, Yield
  • 270 MPa @Strain 0.200 %, Temperature 871 °C
  • Tensile Strength, Yield
  • 313 MPa @Strain 0.200 %, Temperature 816 °C
  • Elongation at Break
  • 11 %
  • Elongation at Break
  • 17 % @Temperature 816 °C
  • Elongation at Break
  • 18 % @Temperature 871 °C
  • Elongation at Break
  • 22 % @Temperature 1150 °C
  • Elongation at Break
  • 36 % @Temperature 982 °C
  • Elongation at Break
  • 44 % @Temperature 1090 °C
  • Modulus of Elasticity
  • 214 GPa
  • Modulus of Elasticity
  • 210 GPa @Diameter 15.9 mm, Temperature 23.0 °C
  • Izod Impact Unnotched
  • 84.0 J @Thickness 12.7 mm
  • Charpy Impact
  • 8.00 J @Temperature 23.0 °C
  • Charpy Impact
  • 20.0 J @Temperature 538 - 816 °C
  • Charpy Impact, Unnotched
  • 88.0 J
  • Charpy Impact, Unnotched
  • 98.0 J @Temperature 22.2 °C
  • Charpy Impact, Unnotched
  • 110 J @Temperature 538 °C
  • Charpy Impact, Unnotched
  • 157 J @Temperature 677 °C
  • Charpy Impact, Unnotched
  • 171 J @Temperature 816 °C

  • Thermal Properties
  • CTE, linear
  • 13.9 µm/m-°C @Temperature 0.000 - 100 °C
  • CTE, linear
  • 14.1 µm/m-°C @Temperature 0.000 - 200 °C
  • CTE, linear
  • 14.5 µm/m-°C @Temperature 0.000 - 300 °C
  • CTE, linear
  • 14.7 µm/m-°C @Temperature 0.000 - 400 °C
  • CTE, linear
  • 15.0 µm/m-°C @Temperature 0.000 - 500 °C
  • CTE, linear
  • 15.3 µm/m-°C @Temperature 0.000 - 600 °C
  • CTE, linear
  • 15.8 µm/m-°C @Temperature 0.000 - 700 °C
  • CTE, linear
  • 16.3 µm/m-°C @Temperature 0.000 - 800 °C
  • CTE, linear
  • 16.9 µm/m-°C @Temperature 0.000 - 900 °C
  • CTE, linear
  • 17.4 µm/m-°C @Temperature 0.000 - 1000 °C
  • Specific Heat Capacity
  • 0.423 J/g-°C
  • Thermal Conductivity
  • 14.85 W/m-K
  • Melting Point
  • 1265 - 1354 °C
  • Solidus
  • 1265 °C
  • Liquidus
  • 1354 °C

  • Optical Properties
  • Reflection Coefficient, Visible (0-1)
  • 0.57 - 0.70

  • Component Elements Properties
  • Carbon, C
  • 0.90 - 1.4 %
  • Chromium, Cr
  • 28 - 32 %
  • Cobalt, Co
  • 50 - 67 %
  • Iron, Fe
  • <= 3.0 %
  • Manganese, Mn
  • <= 2.0 %
  • Molybdenum, Mo
  • <= 1.5 %
  • Nickel, Ni
  • <= 3.0 %
  • Silicon, Si
  • <= 2.0 %
  • Tungsten, W
  • 3.5 - 5.5 %

  • Electrical Properties
  • Electrical Resistivity
  • 0.0000910 ohm-cm @Temperature 22.0 °C
  • Magnetic Permeability
  • <= 1.20 @Temperature 22.0 °C

Alternative products

ShipsFor-Sale.com is a renowned company specializing in the sale of ships. With years of experience in the maritime industry, they have established themselves as a trusted platform for buyers and sellers worldwide. Offering an extensive range of vessels, including cargo ships, tankers, fishing boats, and luxury yachts, shipsforsale. Their team of knowledgeable professionals provides expert guidance throughout the buying and selling process, ensuring smooth transactions and customer satisfaction. Whether you are a seasoned ship owner or a first-time buyer, ShipsFor-Sale.com offers a comprehensive selection of vessels and a seamless online experience, making them the go-to destination for ship sales.

Andrey Kutuzov

University of Córdoba (Spain), email: [email protected]

1 prices for Kennametal Stellite Stellite® 6B solution heat-treated at 1232°C, 1.6 mm thick sheet

Seller from Ankara – 2021-05-20:

Seller from Ankara work with company: 3M, Solvay, SABIC Innovative Plastics (GE Plastics), ALIMEX GmbH

Price: $1741 per MT

Share on Pinterest
Share on LinkedIn
Share on Reddit

Would you like to sell Kennametal Stellite Stellite® 6B solution heat-treated at 1232°C, 1.6 mm thick sheet?

Plastic warehouse

Find a direct plastic supplier if you're interested in a supplier or Distillery in Singapore open-nearme.com