AK Steel NITRONIC® 30 Austenitic Stainless Steel

Seller in Nanjing price: $1761 per MT

AK Steel NITRONIC® 30 Austenitic Stainless Steel in Stainless Steel

  • Mechanical Properties
  • Hardness, Rockwell B
  • 95
  • Hardness, Rockwell B
  • 92.5 @Temperature 23.9 °C
  • Hardness, Rockwell B
  • 96.5 @Temperature 23.9 °C
  • Hardness, Rockwell B
  • 92 @Thickness 22.2 mm
  • Hardness, Rockwell B
  • 93 @Thickness 1.63 mm
  • Hardness, Rockwell B
  • 93 @Thickness 1.63 mm
  • Hardness, Rockwell B
  • 93.5 @Thickness 3.15 mm
  • Hardness, Rockwell B
  • 94 @Thickness 0.813 mm
  • Hardness, Rockwell B
  • 94 @Thickness 0.813 mm
  • Hardness, Rockwell B
  • 94 @Thickness 9.52 mm
  • Hardness, Rockwell C
  • 31
  • Hardness, Rockwell C
  • 37
  • Hardness, Rockwell C
  • 43
  • Hardness, Rockwell C
  • 45
  • Hardness, Rockwell C
  • 33.5 @Thickness 4.762 mm
  • Hardness, Rockwell C
  • 33.5 @Thickness 4.762 mm
  • Hardness, Rockwell C
  • 34 @Thickness 6.35 mm
  • Hardness, Rockwell C
  • 34 @Thickness 6.35 mm
  • Tensile Strength, Ultimate
  • 862 MPa
  • Tensile Strength, Ultimate
  • 1034 MPa
  • Tensile Strength, Ultimate
  • 1193 MPa
  • Tensile Strength, Ultimate
  • 1338 MPa
  • Tensile Strength, Ultimate
  • 1467 MPa
  • Tensile Strength, Ultimate
  • 417 MPa @Temperature 538 °C
  • Tensile Strength, Ultimate
  • 439 MPa @Temperature 482 °C
  • Tensile Strength, Ultimate
  • 459 MPa @Temperature 538 °C
  • Tensile Strength, Ultimate
  • 460 MPa @Temperature 427 °C
  • Tensile Strength, Ultimate
  • 480 MPa @Temperature 371 °C
  • Tensile Strength, Ultimate
  • 485 MPa @Temperature 482 °C
  • Tensile Strength, Ultimate
  • 487 MPa @Temperature 260 °C
  • Tensile Strength, Ultimate
  • 488 MPa @Temperature 316 °C
  • Tensile Strength, Ultimate
  • 496 MPa @Temperature 204 °C
  • Tensile Strength, Ultimate
  • 506 MPa @Temperature 427 °C
  • Tensile Strength, Ultimate
  • 529 MPa @Temperature 371 °C
  • Tensile Strength, Ultimate
  • 539 MPa @Temperature 149 °C
  • Tensile Strength, Ultimate
  • 547 MPa @Temperature 316 °C
  • Tensile Strength, Ultimate
  • 547 MPa @Temperature 260 °C
  • Tensile Strength, Ultimate
  • 561 MPa @Temperature 204 °C
  • Tensile Strength, Ultimate
  • 598 MPa @Temperature 149 °C
  • Tensile Strength, Ultimate
  • 630 MPa @Temperature 93.3 °C
  • Tensile Strength, Ultimate
  • 692 MPa @Temperature 93.3 °C
  • Tensile Strength, Ultimate
  • 845 MPa @Temperature 23.9 °C
  • Tensile Strength, Ultimate
  • 850 MPa @Temperature 23.9 °C
  • Tensile Strength, Ultimate
  • 689 MPa @Thickness 1.63 mm
  • Tensile Strength, Ultimate
  • 711 MPa @Thickness 1.63 mm
  • Tensile Strength, Ultimate
  • 786 MPa @Thickness 9.52 mm
  • Tensile Strength, Ultimate
  • 811 MPa @Thickness 3.15 mm
  • Tensile Strength, Ultimate
  • 825 MPa @Thickness 0.813 mm
  • Tensile Strength, Ultimate
  • 827 MPa @Thickness 50.8 mm
  • Tensile Strength, Ultimate
  • 840 MPa @Thickness 0.813 mm
  • Tensile Strength, Ultimate
  • 855 MPa @Thickness 22.2 mm
  • Tensile Strength, Ultimate
  • 998 MPa @Thickness 6.35 mm
  • Tensile Strength, Ultimate
  • 1011 MPa @Thickness 6.35 mm
  • Tensile Strength, Ultimate
  • 1020 MPa @Thickness 4.762 mm
  • Tensile Strength, Ultimate
  • 1025 MPa @Thickness 4.762 mm
  • Tensile Strength, Yield
  • 345 MPa @Strain 0.200 %
  • Tensile Strength, Yield
  • 358 MPa @Strain 0.200 %
  • Tensile Strength, Yield
  • 393 MPa @Strain 0.200 %
  • Tensile Strength, Yield
  • 393 MPa @Strain 0.200 %
  • Tensile Strength, Yield
  • 593 MPa @Strain 0.200 %
  • Tensile Strength, Yield
  • 702 MPa @Strain 0.200 %
  • Tensile Strength, Yield
  • 717 MPa @Strain 0.200 %
  • Tensile Strength, Yield
  • 759 MPa @Strain 0.200 %
  • Tensile Strength, Yield
  • 768 MPa @Strain 0.200 %
  • Tensile Strength, Yield
  • 779 MPa @Strain 0.200 %
  • Tensile Strength, Yield
  • 979 MPa @Strain 0.200 %
  • Tensile Strength, Yield
  • 1186 MPa @Strain 0.200 %
  • Tensile Strength, Yield
  • 131 MPa @Strain 0.200 %, Temperature 538 °C
  • Tensile Strength, Yield
  • 155 MPa @Strain 0.200 %, Temperature 482 °C
  • Tensile Strength, Yield
  • 157 MPa @Strain 0.200 %, Temperature 427 °C
  • Tensile Strength, Yield
  • 168 MPa @Strain 0.200 %, Temperature 371 °C
  • Tensile Strength, Yield
  • 174 MPa @Strain 0.200 %, Temperature 316 °C
  • Tensile Strength, Yield
  • 182 MPa @Strain 0.200 %, Temperature 260 °C

Alternative products

ShipsFor-Sale.com is a renowned company specializing in the sale of ships. With years of experience in the maritime industry, they have established themselves as a trusted platform for buyers and sellers worldwide. Offering an extensive range of vessels, including cargo ships, tankers, fishing boats, and luxury yachts, lng tanker for sale. Their team of knowledgeable professionals provides expert guidance throughout the buying and selling process, ensuring smooth transactions and customer satisfaction. Whether you are a seasoned ship owner or a first-time buyer, ShipsFor-Sale.com offers a comprehensive selection of vessels and a seamless online experience, making them the go-to destination for ship sales.

Andrey Kutuzov

University of Córdoba (Spain), email: [email protected]

1 prices for AK Steel NITRONIC® 30 Austenitic Stainless Steel

Seller from Nanjing – 2021-07-23:

Seller from Nanjing work with company: 3M, Solvay, SABIC Innovative Plastics (GE Plastics), ALIMEX GmbH

Price: $1761 per MT

Share on Pinterest
Share on LinkedIn
Share on Reddit

Would you like to sell AK Steel NITRONIC® 30 Austenitic Stainless Steel?

Plastic warehouse

Find a direct plastic supplier if you're interested in a supplier or Paper mill in Singapore open-nearme.com