Special Metals INCONEL® 625LCF® Nickel Superalloy (UNS N06626) Annealed 2150°F (1180°C) in Nickel Alloy, Superalloy

  • Physical Properties
  • Density
  • 8.44 g/cc

  • Mechanical Properties
  • Hardness, Rockwell B
  • 84
  • Tensile Strength, Ultimate
  • 769.5 MPa
  • Tensile Strength, Yield
  • 319 MPa @Strain 0.200 %
  • Elongation at Break
  • 63 %
  • Modulus of Elasticity
  • 208 GPa
  • Poissons Ratio
  • 0.28
  • Shear Modulus
  • 81.4 GPa

  • Thermal Properties
  • CTE, linear
  • 12.8 µm/m-°C @Temperature 21.0 - 100 °C
  • CTE, linear
  • 13.3 µm/m-°C @Temperature 21.0 - 300 °C
  • CTE, linear
  • 13.9 µm/m-°C @Temperature 21.0 - 500 °C
  • CTE, linear
  • 14.9 µm/m-°C @Temperature 21.0 - 700 °C
  • Specific Heat Capacity
  • 0.410 J/g-°C
  • Thermal Conductivity
  • 9.70 W/m-K
  • Melting Point
  • 1290 - 1350 °C
  • Solidus
  • 1290 °C
  • Liquidus
  • 1350 °C
  • Maximum Service Temperature, Air
  • 650 °C

  • Component Elements Properties
  • Aluminum, Al
  • <= 0.40 %
  • Carbon, C
  • <= 0.030 %
  • Chromium, Cr
  • 20 - 23 %
  • Cobalt, Co
  • <= 1.0 %
  • Iron, Fe
  • <= 5.0 %
  • Manganese, Mn
  • <= 0.50 %
  • Molybdenum, Mo
  • 8.0 - 10 %
  • Nickel, Ni
  • >= 58 %
  • Niobium, Nb (Columbium, Cb)
  • 3.15 - 4.15 %
  • Nitrogen, N
  • <= 0.020 %
  • Phosphorous, P
  • <= 0.015 %
  • Silicon, Si
  • <= 0.020 %
  • Sulfur, S
  • <= 0.015 %
  • Titanium, Ti
  • <= 0.40 %

  • Electrical Properties
  • Electrical Resistivity
  • 0.000132 ohm-cm
  • Magnetic Permeability
  • 1.0006

Alternative products

ShipsFor-Sale.com is a renowned company specializing in the sale of ships. With years of experience in the maritime industry, they have established themselves as a trusted platform for buyers and sellers worldwide. Offering an extensive range of vessels, including cargo ships, tankers, fishing boats, and luxury yachts, cargo ship for sale in turkey. Their team of knowledgeable professionals provides expert guidance throughout the buying and selling process, ensuring smooth transactions and customer satisfaction. Whether you are a seasoned ship owner or a first-time buyer, ShipsFor-Sale.com offers a comprehensive selection of vessels and a seamless online experience, making them the go-to destination for ship sales.

Andrey Kutuzov

University of Córdoba (Spain), email: a.kutuzov@plastic-price.com

4 prices for Special Metals INCONEL® 625LCF® Nickel Superalloy (UNS N06626) Annealed 2150°F (1180°C)

Seller from Tianjin – 2021-07-05:

Seller from Tianjin work with company: 3M, Solvay, SABIC Innovative Plastics (GE Plastics), ALIMEX GmbH

Price: $1655 per MT

Seller from Hāora – 2021-07-14:

Seller from Hāora work with company: Solvay, RTP Company, SABIC Innovative Plastics (GE Plastics), ALIMEX GmbH

Price: $1820 per MT

Seller from Bogotá – 2021-03-03:

Seller from Bogotá work with company: Solvay, Teknor Apex Company, SABIC Innovative Plastics (GE Plastics), BASF

Price: $1458 per MT

Seller from Abidjan – 2021-04-16:

Seller from Abidjan work with company: RTP Company, Teknor Apex Company, SABIC Innovative Plastics (GE Plastics), ALIMEX GmbH

Price: $1633 per MT

Share on Pinterest
Share on LinkedIn
Share on Reddit

Would you like to sell Special Metals INCONEL® 625LCF® Nickel Superalloy (UNS N06626) Annealed 2150°F (1180°C)?

Plastic warehouse

Find a direct plastic supplier if you're interested in a supplier or Retreat center in Singapore open-nearme.com