Special Metals INCONEL® 625LCF® Nickel Superalloy (UNS N06626) Annealed + 5% Cold Work

Seller in Toronto price: $2384 per MT
Seller in Xi’an price: $2572 per MT

Special Metals INCONEL® 625LCF® Nickel Superalloy (UNS N06626) Annealed + 5% Cold Work in Nickel Alloy, Superalloy

  • Physical Properties
  • Density
  • 8.44 g/cc

  • Mechanical Properties
  • Tensile Strength, Ultimate
  • 951 MPa
  • Tensile Strength, Yield
  • 563 MPa @Strain 0.200 %
  • Elongation at Break
  • 46 %
  • Modulus of Elasticity
  • 208 GPa
  • Poissons Ratio
  • 0.28
  • Shear Modulus
  • 81.4 GPa

  • Thermal Properties
  • CTE, linear
  • 12.8 µm/m-°C @Temperature 21.0 - 100 °C
  • CTE, linear
  • 13.3 µm/m-°C @Temperature 21.0 - 300 °C
  • CTE, linear
  • 13.9 µm/m-°C @Temperature 21.0 - 500 °C
  • CTE, linear
  • 14.9 µm/m-°C @Temperature 21.0 - 700 °C
  • Specific Heat Capacity
  • 0.410 J/g-°C
  • Thermal Conductivity
  • 9.70 W/m-K
  • Melting Point
  • 1290 - 1350 °C
  • Solidus
  • 1290 °C
  • Liquidus
  • 1350 °C
  • Maximum Service Temperature, Air
  • 650 °C

  • Component Elements Properties
  • Aluminum, Al
  • <= 0.40 %
  • Carbon, C
  • <= 0.030 %
  • Chromium, Cr
  • 20 - 23 %
  • Cobalt, Co
  • <= 1.0 %
  • Iron, Fe
  • <= 5.0 %
  • Manganese, Mn
  • <= 0.50 %
  • Molybdenum, Mo
  • 8.0 - 10 %
  • Nickel, Ni
  • >= 58 %
  • Niobium, Nb (Columbium, Cb)
  • 3.15 - 4.15 %
  • Nitrogen, N
  • <= 0.020 %
  • Phosphorous, P
  • <= 0.015 %
  • Silicon, Si
  • <= 0.020 %
  • Sulfur, S
  • <= 0.015 %
  • Titanium, Ti
  • <= 0.40 %

  • Electrical Properties
  • Electrical Resistivity
  • 0.000132 ohm-cm
  • Magnetic Permeability
  • 1.0006

Alternative products

ShipsFor-Sale.com is a renowned company specializing in the sale of ships. With years of experience in the maritime industry, they have established themselves as a trusted platform for buyers and sellers worldwide. Offering an extensive range of vessels, including cargo ships, tankers, fishing boats, and luxury yachts, chemical tankers for sale. Their team of knowledgeable professionals provides expert guidance throughout the buying and selling process, ensuring smooth transactions and customer satisfaction. Whether you are a seasoned ship owner or a first-time buyer, ShipsFor-Sale.com offers a comprehensive selection of vessels and a seamless online experience, making them the go-to destination for ship sales.

Andrey Kutuzov

University of Córdoba (Spain), email: a.kutuzov@plastic-price.com

2 prices for Special Metals INCONEL® 625LCF® Nickel Superalloy (UNS N06626) Annealed + 5% Cold Work

Seller from Toronto – 2021-03-16:

Seller from Toronto work with company: Solvay, Dow Corning, SABIC Innovative Plastics (GE Plastics), ALIMEX GmbH

Price: $2384 per MT

Seller from Xi’an – 2021-04-18:

Seller from Xi’an work with company: 3M, Solvay, RTP Company, SABIC Innovative Plastics (GE Plastics)

Price: $2572 per MT

Share on Pinterest
Share on LinkedIn
Share on Reddit

Would you like to sell Special Metals INCONEL® 625LCF® Nickel Superalloy (UNS N06626) Annealed + 5% Cold Work?

Plastic warehouse

Find a direct plastic supplier if you're interested in a supplier or Food products supplier in Singapore open-nearme.com