Haynes Hastelloy® C-22HSâ„¢ Nickel Alloy Plate and Bar, Hot-rolled, Solution Annealed

Seller in Ahmadābād price: $2344 per MT

Haynes Hastelloy® C-22HSâ„¢ Nickel Alloy Plate and Bar, Hot-rolled, Solution Annealed in Nickel Alloy

  • Physical Properties
  • Density
  • 8.60 g/cc
  • Density
  • 8.64 g/cc

  • Mechanical Properties
  • Hardness, Rockwell B
  • 88
  • Hardness, Rockwell B
  • 92
  • Tensile Strength, Ultimate
  • 628 MPa @Temperature 600 °C
  • Tensile Strength, Ultimate
  • 652 MPa @Temperature 500 °C
  • Tensile Strength, Ultimate
  • 677 MPa @Temperature 400 °C
  • Tensile Strength, Ultimate
  • 695 MPa @Temperature 300 °C
  • Tensile Strength, Ultimate
  • 721 MPa @Temperature 200 °C
  • Tensile Strength, Ultimate
  • 767 MPa @Temperature 100 °C
  • Tensile Strength, Ultimate
  • 806 MPa @Temperature 25.0 °C
  • Tensile Strength, Yield
  • 223 MPa @Strain 0.200 %, Temperature 600 °C
  • Tensile Strength, Yield
  • 241 MPa @Strain 0.200 %, Temperature 500 °C
  • Tensile Strength, Yield
  • 255 MPa @Strain 0.200 %, Temperature 400 °C
  • Tensile Strength, Yield
  • 263 MPa @Strain 0.200 %, Temperature 300 °C
  • Tensile Strength, Yield
  • 288 MPa @Strain 0.200 %, Temperature 200 °C
  • Tensile Strength, Yield
  • 329 MPa @Strain 0.200 %, Temperature 100 °C
  • Tensile Strength, Yield
  • 376 MPa @Strain 0.200 %, Temperature 25.0 °C
  • Elongation at Break
  • 62.3 % @Temperature 25.0 °C
  • Elongation at Break
  • 65.9 % @Temperature 200 °C
  • Elongation at Break
  • 66.7 % @Temperature 100 °C
  • Elongation at Break
  • 68.8 % @Temperature 300 °C
  • Elongation at Break
  • 69.3 % @Temperature 500 °C
  • Elongation at Break
  • 69.5 % @Temperature 400 °C
  • Elongation at Break
  • 70.6 % @Temperature 600 °C
  • Reduction of Area
  • 69.1 % @Temperature 600 °C
  • Reduction of Area
  • 70.9 % @Temperature 500 °C
  • Reduction of Area
  • 73 % @Temperature 400 °C
  • Reduction of Area
  • 75.2 % @Temperature 300 °C
  • Reduction of Area
  • 77.3 % @Temperature 200 °C
  • Reduction of Area
  • 77.5 % @Temperature 25.0 °C
  • Reduction of Area
  • 78 % @Temperature 100 °C
  • Modulus of Elasticity
  • 181 GPa @Temperature 600 °C
  • Modulus of Elasticity
  • 195 GPa @Temperature 500 °C
  • Modulus of Elasticity
  • 205 GPa @Temperature 400 °C
  • Modulus of Elasticity
  • 209 GPa @Temperature 300 °C
  • Modulus of Elasticity
  • 211 GPa @Temperature 200 °C
  • Modulus of Elasticity
  • 218 GPa @Temperature 100 °C
  • Modulus of Elasticity
  • 223 GPa @Temperature 25.0 °C

  • Thermal Properties
  • CTE, linear
  • 11.6 µm/m-°C @Temperature 25.0 - 100 °C
  • CTE, linear
  • 12.0 µm/m-°C @Temperature 25.0 - 200 °C
  • CTE, linear
  • 12.4 µm/m-°C @Temperature 25.0 - 300 °C
  • CTE, linear
  • 12.7 µm/m-°C @Temperature 25.0 - 400 °C
  • CTE, linear
  • 13.1 µm/m-°C @Temperature 25.0 - 500 °C
  • CTE, linear
  • 13.3 µm/m-°C @Temperature 25.0 - 600 °C
  • Specific Heat Capacity
  • 0.412 J/g-°C @Temperature 25.0 °C
  • Specific Heat Capacity
  • 0.434 J/g-°C @Temperature 100 °C
  • Specific Heat Capacity
  • 0.451 J/g-°C @Temperature 200 °C
  • Specific Heat Capacity
  • 0.465 J/g-°C @Temperature 300 °C
  • Specific Heat Capacity
  • 0.477 J/g-°C @Temperature 400 °C
  • Specific Heat Capacity
  • 0.488 J/g-°C @Temperature 500 °C
  • Specific Heat Capacity
  • 0.504 J/g-°C @Temperature 600 °C
  • Thermal Conductivity
  • 11.8 W/m-K @Temperature 25.0 °C
  • Thermal Conductivity
  • 13.5 W/m-K @Temperature 100 °C
  • Thermal Conductivity
  • 15.4 W/m-K @Temperature 200 °C
  • Thermal Conductivity
  • 17.1 W/m-K @Temperature 300 °C
  • Thermal Conductivity
  • 18.6 W/m-K @Temperature 400 °C
  • Thermal Conductivity
  • 20.5 W/m-K @Temperature 500 °C
  • Thermal Conductivity
  • 22.4 W/m-K @Temperature 600 °C
  • Melting Point
  • 1304 - 1368 °C
  • Solidus
  • 1304 °C
  • Liquidus
  • 1368 °C

  • Electrical Properties
  • Electrical Resistivity
  • 0.0000980 ohm-cm @Temperature 25.0 °C
  • Electrical Resistivity
  • 0.000100 ohm-cm @Temperature 100 °C
  • Electrical Resistivity
  • 0.000104 ohm-cm @Temperature 200 °C
  • Electrical Resistivity
  • 0.000108 ohm-cm @Temperature 300 °C
  • Electrical Resistivity
  • 0.000112 ohm-cm @Temperature 400 °C
  • Electrical Resistivity
  • 0.000115 ohm-cm @Temperature 500 °C
  • Electrical Resistivity
  • 0.000117 ohm-cm @Temperature 600 °C

  • Processing Properties
  • Annealing Temperature
  • 1079 °C

Alternative products

ShipsFor-Sale.com is a renowned company specializing in the sale of ships. With years of experience in the maritime industry, they have established themselves as a trusted platform for buyers and sellers worldwide. Offering an extensive range of vessels, including cargo ships, tankers, fishing boats, and luxury yachts, oil tankers for sale. Their team of knowledgeable professionals provides expert guidance throughout the buying and selling process, ensuring smooth transactions and customer satisfaction. Whether you are a seasoned ship owner or a first-time buyer, ShipsFor-Sale.com offers a comprehensive selection of vessels and a seamless online experience, making them the go-to destination for ship sales.

Andrey Kutuzov

University of Córdoba (Spain), email: [email protected]

1 prices for Haynes Hastelloy® C-22HSâ„¢ Nickel Alloy Plate and Bar, Hot-rolled, Solution Annealed

Seller from Ahmadābād – 2021-06-06:

Seller from Ahmadābād work with company: Solvay, RTP Company, SABIC Innovative Plastics (GE Plastics), ALIMEX GmbH

Price: $2344 per MT

Share on Pinterest
Share on LinkedIn
Share on Reddit

Would you like to sell Haynes Hastelloy® C-22HSâ„¢ Nickel Alloy Plate and Bar, Hot-rolled, Solution Annealed?

Plastic warehouse

Find a direct plastic supplier if you're interested in a supplier or Custom t-shirt store in Singapore open-nearme.com