Special Metals INCONEL® 690 Nickel Superalloy, Hot Rolled Flat, 0.62 inch (16 mm) Diameter

Seller in Beijing price: $2032 per MT
Seller in Atlanta price: $2090 per MT
Seller in Mexico City price: $2138 per MT
Seller in Saint Petersburg price: $2141 per MT

Special Metals INCONEL® 690 Nickel Superalloy, Hot Rolled Flat, 0.62 inch (16 mm) Diameter in Nickel Alloy, Superalloy

  • Physical Properties
  • Density
  • 8.19 g/cc

  • Mechanical Properties
  • Tensile Strength, Ultimate
  • 738 MPa
  • Tensile Strength, Yield
  • 372 MPa @Strain 0.200 %
  • Elongation at Break
  • 44 %
  • Modulus of Elasticity
  • 211 GPa
  • Poissons Ratio
  • 0.289
  • Shear Modulus
  • 81.8 GPa

  • Thermal Properties
  • CTE, linear
  • 14.06 µm/m-°C @Temperature 24.0 - 100 °C
  • CTE, linear
  • 14.53 µm/m-°C @Temperature 24.0 - 300 °C
  • CTE, linear
  • 15.19 µm/m-°C @Temperature 24.0 - 500 °C
  • CTE, linear
  • 17.41 µm/m-°C @Temperature 20.0 - 1000 °C
  • Specific Heat Capacity
  • 0.450 J/g-°C
  • Thermal Conductivity
  • 13.5 W/m-K
  • Melting Point
  • 1343 - 1377 °C
  • Solidus
  • 1343 °C
  • Liquidus
  • 1377 °C

  • Component Elements Properties
  • Carbon, C
  • <= 0.050 %
  • Chromium, Cr
  • 27 - 31 %
  • Copper, Cu
  • 0.50 %
  • Iron, Fe
  • 7.0 - 11 %
  • Manganese, Mn
  • <= 0.50 %
  • Nickel, Ni
  • >= 58 %
  • Silicon, Si
  • <= 0.50 %
  • Sulfur, S
  • <= 0.15 %

  • Electrical Properties
  • Electrical Resistivity
  • 0.0001148 ohm-cm
  • Magnetic Permeability
  • 1.001

Alternative products

ShipsFor-Sale.com is a renowned company specializing in the sale of ships. With years of experience in the maritime industry, they have established themselves as a trusted platform for buyers and sellers worldwide. Offering an extensive range of vessels, including cargo ships, tankers, fishing boats, and luxury yachts, lng tankers for sale qld. Their team of knowledgeable professionals provides expert guidance throughout the buying and selling process, ensuring smooth transactions and customer satisfaction. Whether you are a seasoned ship owner or a first-time buyer, ShipsFor-Sale.com offers a comprehensive selection of vessels and a seamless online experience, making them the go-to destination for ship sales.

Andrey Kutuzov

University of Córdoba (Spain), email: [email protected]

4 prices for Special Metals INCONEL® 690 Nickel Superalloy, Hot Rolled Flat, 0.62 inch (16 mm) Diameter

Seller from Beijing – 2021-03-10:

Seller from Beijing work with company: Solvay, RTP Company, SABIC Innovative Plastics (GE Plastics), ALIMEX GmbH

Price: $2032 per MT

Seller from Atlanta – 2021-06-15:

Seller from Atlanta work with company: RTP Company, Teknor Apex Company, SABIC Innovative Plastics (GE Plastics), ALIMEX GmbH

Price: $2090 per MT

Seller from Mexico City – 2021-05-12:

Seller from Mexico City work with company: Solvay, Exxon Chemical, SABIC Innovative Plastics (GE Plastics), ALIMEX GmbH

Price: $2138 per MT

Seller from Saint Petersburg – 2021-05-19:

Seller from Saint Petersburg work with company: Solvay, SABIC Innovative Plastics (GE Plastics), Lehmann & Voss & Co., ALIMEX GmbH

Price: $2141 per MT

Share on Pinterest
Share on LinkedIn
Share on Reddit

Would you like to sell Special Metals INCONEL® 690 Nickel Superalloy, Hot Rolled Flat, 0.62 inch (16 mm) Diameter?

Plastic warehouse

Find a direct plastic supplier if you're interested in a supplier or Oriental medicine store in Singapore open-nearme.com