  • Physical Properties
  • Density
  • 8.19 g/cc

  • Mechanical Properties
  • Hardness, Rockwell C
  • 24
  • Tensile Strength, Ultimate
  • 1120 MPa
  • Tensile Strength, Yield
  • 827 MPa @Strain 0.200 %
  • Elongation at Break
  • 31 %
  • Modulus of Elasticity
  • 205 GPa
  • Poissons Ratio
  • 0.284
  • Shear Modulus
  • 80.0 GPa

  • Thermal Properties
  • CTE, linear
  • 12.15 µm/m-°C @Temperature 21.0 - 93.0 °C
  • CTE, linear
  • 13.77 µm/m-°C @Temperature 21.0 - 316 °C
  • CTE, linear
  • 14.4 µm/m-°C @Temperature 21.0 - 538 °C
  • Specific Heat Capacity
  • 0.435 J/g-°C
  • Thermal Conductivity
  • 11.1 W/m-K
  • Melting Point
  • 1260 - 1335 °C
  • Solidus
  • 1260 °C
  • Liquidus
  • 1335 °C

  • Component Elements Properties
  • Aluminum, Al
  • 0.20 - 0.80 %
  • Boron, B
  • <= 0.0060 %
  • Carbon, C
  • <= 0.050 %
  • Chromium, Cr
  • 17 - 21 %
  • Cobalt, Co
  • <= 1.0 %
  • Copper, Cu
  • <= 0.30 %
  • Iron, Fe
  • 19 %
  • Manganese, Mn
  • <= 0.35 %
  • Molybdenum, Mo
  • 2.8 - 3.3 %
  • Nickel, Ni
  • 50 - 55 %
  • Niobium, Nb (Columbium, Cb)
  • 4.75 - 5.25 %
  • Nitrogen, N
  • <= 0.010 %
  • Phosphorous, P
  • <= 0.015 %
  • Silicon, Si
  • <= 0.35 %
  • Sulfur, S
  • <= 0.0020 %
  • Titanium, Ti
  • 0.65 - 1.15 %

  • Electrical Properties
  • Electrical Resistivity
  • 0.000125 ohm-cm
  • Magnetic Permeability
  • 1.0013
  • Curie Temperature
  • <= -197 °C

Alternative products

ShipsFor-Sale.com is a renowned company specializing in the sale of ships. With years of experience in the maritime industry, they have established themselves as a trusted platform for buyers and sellers worldwide. Offering an extensive range of vessels, including cargo ships, tankers, fishing boats, and luxury yachts, chemical tankers for sale. Their team of knowledgeable professionals provides expert guidance throughout the buying and selling process, ensuring smooth transactions and customer satisfaction. Whether you are a seasoned ship owner or a first-time buyer, ShipsFor-Sale.com offers a comprehensive selection of vessels and a seamless online experience, making them the go-to destination for ship sales.

Andrey Kutuzov

University of Córdoba (Spain), email: [email protected]

6 prices for Special Metals INCONEL® 718SPFâ„¢ Nickel Superalloy, Annealed

Seller from Khartoum – 2021-07-28:

Seller from Khartoum work with company: 3M, RTP Company, SABIC Innovative Plastics (GE Plastics), ALIMEX GmbH

Price: $1637 per MT

Seller from Dhaka – 2021-06-21:

Seller from Dhaka work with company: 3M, RTP Company, SABIC Innovative Plastics (GE Plastics), ALIMEX GmbH

Price: $1943 per MT

Seller from Toronto – 2021-03-30:

Seller from Toronto work with company: 3M, Solvay, SABIC Innovative Plastics (GE Plastics), ALIMEX GmbH

Price: $1825 per MT

Seller from Melbourne – 2021-06-19:

Seller from Melbourne work with company: 3M, RTP Company, SABIC Innovative Plastics (GE Plastics), ALIMEX GmbH

Price: $1783 per MT

Seller from Jakarta – 2021-05-02:

Seller from Jakarta work with company: Solvay, Teknor Apex Company, SABIC Innovative Plastics (GE Plastics), ALIMEX GmbH

Price: $1661 per MT

Seller from Lahore – 2021-04-28:

Seller from Lahore work with company: Solvay, RTP Company, SABIC Innovative Plastics (GE Plastics), ALIMEX GmbH

Price: $1650 per MT

Share on Pinterest
Share on LinkedIn
Share on Reddit

Would you like to sell Special Metals INCONEL® 718SPFâ„¢ Nickel Superalloy, Annealed?

Plastic warehouse

Find a direct plastic supplier if you're interested in a supplier or Pizza restaurant in Singapore open-nearme.com