Seller in Hanoi price: $2091 per MT
Seller in Toronto price: $2058 per MT
Seller in Madrid price: $1733 per MT
Special Metals UDIMET® alloy 520 Superalloy in Nickel Alloy, Superalloy
FOLLOW US ON
Physical Properties
Density
8.21 g/cc
Mechanical Properties
Tensile Strength at Break
350 MPa @Temperature 950 °C
Tensile Strength at Break
1150 MPa @Temperature 700 °C
Tensile Strength at Break
1250 MPa @Temperature 400 °C
Tensile Strength at Break
1300 MPa @Temperature 50.0 °C
Tensile Strength, Yield
500 MPa @Strain 0.200 %, Temperature 850 °C
Tensile Strength, Yield
700 MPa @Strain 0.200 %, Temperature 700 °C
Tensile Strength, Yield
850 MPa @Strain 0.200 %, Temperature 50.0 °C
Tensile Strength, Yield
850 MPa @Strain 0.200 %, Temperature 400 °C
Elongation at Break
100 % @Temperature 50.0 °C
Elongation at Break
100 % @Temperature 400 °C
Elongation at Break
100 % @Temperature 700 °C
Rupture Strength
150 MPa @Temperature 871 °C, Time 3.60e+6 sec
Rupture Strength
230 MPa @Temperature 816 °C, Time 3.60e+6 sec
Rupture Strength
345 MPa @Temperature 760 °C, Time 3.60e+6 sec
Rupture Strength
475 MPa @Temperature 704 °C, Time 3.60e+6 sec
Rupture Strength
585 MPa @Temperature 649 °C, Time 3.60e+6 sec
Thermal Properties
Melting Point
1260 - 1405 °C
Solidus
1260 °C
Liquidus
1405 °C
Component Elements Properties
Aluminum, Al
1.8 - 2.3 %
Boron, B
0.0040 - 0.010 %
Carbon, C
0.020 - 0.060 %
Chromium, Cr
18 - 20 %
Cobalt, Co
11 - 14 %
Molybdenum, Mo
5.5 - 7.0 %
Nickel, Ni
52.18 - 59.976 %
Titanium, Ti
2.9 - 3.25 %
Tungsten, W
0.80 - 1.2 %
Alternative products
ShipsFor-Sale.com is a renowned company specializing in the sale of ships. With years of experience in the maritime industry, they have established themselves as a trusted platform for buyers and sellers worldwide. Offering an extensive range of vessels, including cargo ships, tankers, fishing boats, and luxury yachts, retired cruise ships for sale. Their team of knowledgeable professionals provides expert guidance throughout the buying and selling process, ensuring smooth transactions and customer satisfaction. Whether you are a seasoned ship owner or a first-time buyer, ShipsFor-Sale.com offers a comprehensive selection of vessels and a seamless online experience, making them the go-to destination for ship sales.
3 prices for Special Metals UDIMET® alloy 520 Superalloy
Seller from Hanoi – 2021-04-07:
Seller from Hanoi work with company: Solvay, Teknor Apex Company, SABIC Innovative Plastics (GE Plastics), ALIMEX GmbH
Price: $2091 per MT
Seller from Toronto – 2021-05-10:
Seller from Toronto work with company: Solvay, SABIC Innovative Plastics (GE Plastics), Dow Chemical, ALIMEX GmbH
Price: $2058 per MT
Seller from Madrid – 2021-04-13:
Seller from Madrid work with company: 3M, Solvay, RTP Company, SABIC Innovative Plastics (GE Plastics)
Price: $1733 per MT