  • Physical Properties
  • Density
  • 1.25 g/cc
  • Density
  • 1.47 g/cc
  • Water Absorption
  • 5.0 % @Thickness 2.00 mm
  • Moisture Absorption
  • 1.50 % @Thickness 2.00 mm
  • Viscosity
  • 40000 cP @Shear Rate 5000 1/s, Temperature 315 °C
  • Viscosity
  • 71000 cP @Shear Rate 5000 1/s, Temperature 295 °C
  • Viscosity
  • 94000 cP @Shear Rate 500 1/s, Temperature 315 °C
  • Viscosity
  • 127000 cP @Shear Rate 5000 1/s, Temperature 275 °C
  • Viscosity
  • 189000 cP @Shear Rate 500 1/s, Temperature 295 °C
  • Viscosity
  • 383000 cP @Shear Rate 500 1/s, Temperature 275 °C
  • Viscosity Test
  • 140 cm³/g
  • Linear Mold Shrinkage, Flow
  • 0.0040 cm/cm
  • Linear Mold Shrinkage, Transverse
  • 0.011 cm/cm

  • Mechanical Properties
  • Tensile Strength at Break
  • 97.0 MPa
  • Tensile Strength at Break
  • 160 MPa
  • Tensile Stress
  • 23.4 MPa @Strain 0.570 %, Temperature 90.0 °C
  • Tensile Stress
  • 23.7 MPa @Strain 0.440 %, Temperature 40.0 °C
  • Tensile Stress
  • 25.0 MPa @Strain 0.240 %, Temperature 0.000 °C
  • Tensile Stress
  • 25.0 MPa @Strain 0.500 %, Temperature 90.0 °C
  • Tensile Stress
  • 25.2 MPa @Strain 0.700 %, Temperature 150 °C
  • Tensile Stress
  • 25.4 MPa @Strain 0.350 %, Temperature 23.0 °C
  • Tensile Stress
  • 27.3 MPa @Strain 0.220 %, Temperature -20.0 °C
  • Tensile Stress
  • 36.6 MPa @Strain 0.800 %, Temperature 90.0 °C
  • Tensile Stress
  • 45.9 MPa @Strain 1.10 %, Temperature 90.0 °C
  • Tensile Stress
  • 53.0 MPa @Strain 2.28 %, Temperature 90.0 °C
  • Tensile Stress
  • 53.8 MPa @Strain 1.40 %, Temperature 90.0 °C
  • Tensile Stress
  • 59.4 MPa @Strain 3.99 %, Temperature 90.0 °C
  • Tensile Stress
  • 59.5 MPa @Strain 2.80 %, Temperature 150 °C
  • Tensile Stress
  • 64.9 MPa @Strain 1.76 %, Temperature 40.0 °C
  • Tensile Stress
  • 65.5 MPa @Strain 4.70 %, Temperature 150 °C
  • Tensile Stress
  • 68.8 MPa @Strain 1.40 %, Temperature 23.0 °C
  • Tensile Stress
  • 75.6 MPa @Strain 3.40 %, Temperature 90.0 °C
  • Tensile Stress
  • 78.4 MPa @Strain 3.08 %, Temperature 40.0 °C
  • Tensile Stress
  • 78.5 MPa @Strain 0.960 %, Temperature 0.000 °C
  • Tensile Stress
  • 84.6 MPa @Strain 0.880 %, Temperature 40.0 °C
  • Tensile Stress
  • 85.4 MPa @Strain 2.45 %, Temperature 23.0 °C
  • Tensile Stress
  • 87.5 MPa @Strain 0.880 %, Temperature -20.0 °C
  • Tensile Stress
  • 108 MPa @Strain 1.10 %, Temperature 23.0 °C
  • Tensile Stress
  • 109 MPa @Strain 1.68 %, Temperature 0.000 °C
  • Tensile Stress
  • 115 MPa @Strain 1.15 %, Temperature 0.000 °C
  • Tensile Stress
  • 116 MPa @Strain 1.54 %, Temperature 40.0 °C
  • Tensile Stress
  • 120 MPa @Strain 1.19 %, Temperature -20.0 °C
  • Tensile Stress
  • 123.9 MPa @Strain 1.20 %, Temperature -40.0 °C
  • Tensile Stress
  • 126 MPa @Strain 2.40 %, Temperature 0.000 °C
  • Tensile Stress
  • 130 MPa @Strain 2.20 %, Temperature 40.0 °C
  • Tensile Stress
  • 138 MPa @Strain 1.76 %, Temperature 23.0 °C
  • Tensile Stress
  • 140 MPa @Strain 1.76 %, Temperature -20.0 °C
  • Tensile Stress
  • 149 MPa @Strain 1.84 %, Temperature 0.000 °C
  • Tensile Stress
  • 149.8 MPa @Strain 1.50 %, Temperature -40.0 °C
  • Tensile Stress
  • 150 MPa @Strain 1.76 %, Temperature -20.0 °C
  • Tensile Stress
  • 172.4 MPa @Strain 1.80 %, Temperature -40.0 °C
  • Tensile Stress
  • 191.7 MPa @Strain 2.10 %, Temperature -40.0 °C
  • Tensile Stress
  • 10.0 MPa @Strain 0.170 %, Time 3600 sec
  • Tensile Stress
  • 10.0 MPa @Strain 0.180 %, Time 36000 sec
  • Tensile Stress
  • 10.0 MPa @Strain 0.210 %, Time 360000 sec
  • Tensile Stress
  • 10.0 MPa @Strain 0.270 %, Time 3.60e+6 sec
  • Elongation at Break
  • 2.2 %
  • Elongation at Break
  • 4.6 %
  • Tensile Modulus
  • 6.50 GPa
  • Tensile Modulus
  • 10.0 GPa
  • Tensile Modulus
  • 2.59 GPa @Temperature 130 °C
  • Tensile Modulus
  • 4.88 GPa @Temperature 70.0 °C
  • Tensile Modulus
  • 7.84 GPa @Temperature -10.0 °C
  • Tensile Modulus
  • 8.55 GPa @Temperature -60.0 °C
  • Tensile Modulus
  • 9.94 GPa @Temperature -110 °C
  • Tensile Modulus
  • 11.2 GPa @Temperature -140 °C

Alternative products

ShipsFor-Sale.com is a renowned company specializing in the sale of ships. With years of experience in the maritime industry, they have established themselves as a trusted platform for buyers and sellers worldwide. Offering an extensive range of vessels, including cargo ships, tankers, fishing boats, and luxury yachts, old cruise ships for sale. Their team of knowledgeable professionals provides expert guidance throughout the buying and selling process, ensuring smooth transactions and customer satisfaction. Whether you are a seasoned ship owner or a first-time buyer, ShipsFor-Sale.com offers a comprehensive selection of vessels and a seamless online experience, making them the go-to destination for ship sales.

Andrey Kutuzov

University of Córdoba (Spain), email: [email protected]

1 prices for DuPont Performance Polymers Minlon® EFE6053 BK413 Nylon 66  (Unverified Data**)

Seller from Tehran – 2021-04-01:

Seller from Tehran work with company: Solvay, RTP Company, SABIC Innovative Plastics (GE Plastics), ALIMEX GmbH

Price: $2581 per MT

Share on Pinterest
Share on LinkedIn
Share on Reddit

Would you like to sell DuPont Performance Polymers Minlon® EFE6053 BK413 Nylon 66  (Unverified Data**)?

Plastic warehouse

Find a direct plastic supplier if you're interested in a supplier or Fortune telling services in Singapore open-nearme.com