  • Physical Properties
  • Density
  • 9.05 g/cc

  • Mechanical Properties
  • Hardness, Brinell
  • 257
  • Hardness, Knoop
  • 286
  • Hardness, Rockwell C
  • 19
  • Hardness, Vickers
  • 78.0 @Temperature 870 °C
  • Hardness, Vickers
  • 140 @Temperature 760 °C
  • Hardness, Vickers
  • 218 @Temperature 650 °C
  • Hardness, Vickers
  • 263 @Temperature 540 °C
  • Hardness, Vickers
  • 271 @Temperature 425 °C
  • Tensile Strength, Ultimate
  • 1325 MPa
  • Tensile Strength, Yield
  • 895 MPa @Strain 0.200 %
  • Elongation at Break
  • 32 %
  • Modulus of Elasticity
  • 229 GPa
  • Modulus of Elasticity
  • 152 GPa @Temperature 1000 °C
  • Modulus of Elasticity
  • 163 GPa @Temperature 900 °C
  • Modulus of Elasticity
  • 172 GPa @Temperature 800 °C
  • Modulus of Elasticity
  • 185 GPa @Temperature 700 °C
  • Modulus of Elasticity
  • 193 GPa @Temperature 600 °C
  • Modulus of Elasticity
  • 199 GPa @Temperature 500 °C
  • Modulus of Elasticity
  • 206 GPa @Temperature 400 °C
  • Modulus of Elasticity
  • 213 GPa @Temperature 300 °C
  • Modulus of Elasticity
  • 219 GPa @Temperature 200 °C
  • Modulus of Elasticity
  • 225 GPa @Temperature 100 °C

  • Thermal Properties
  • CTE, linear
  • 10.8 µm/m-°C @Temperature 25.0 - 100 °C
  • CTE, linear
  • 11.3 µm/m-°C @Temperature 25.0 - 200 °C
  • CTE, linear
  • 11.6 µm/m-°C @Temperature 25.0 - 300 °C
  • CTE, linear
  • 11.9 µm/m-°C @Temperature 25.0 - 400 °C
  • CTE, linear
  • 12.2 µm/m-°C @Temperature 25.0 - 500 °C
  • CTE, linear
  • 12.3 µm/m-°C @Temperature 25.0 - 600 °C
  • CTE, linear
  • 12.4 µm/m-°C @Temperature 25.0 - 650 °C
  • CTE, linear
  • 13.0 µm/m-°C @Temperature 25.0 - 700 °C
  • CTE, linear
  • 13.7 µm/m-°C @Temperature 25.0 - 750 °C
  • CTE, linear
  • 14.0 µm/m-°C @Temperature 25.0 - 800 °C
  • CTE, linear
  • 14.5 µm/m-°C @Temperature 25.0 - 900 °C
  • CTE, linear
  • 15.0 µm/m-°C @Temperature 25.0 - 1000 °C
  • Specific Heat Capacity
  • 0.386 J/g-°C
  • Specific Heat Capacity
  • 0.405 J/g-°C @Temperature 100 °C
  • Specific Heat Capacity
  • 0.419 J/g-°C @Temperature 200 °C
  • Specific Heat Capacity
  • 0.431 J/g-°C @Temperature 300 °C
  • Specific Heat Capacity
  • 0.439 J/g-°C @Temperature 400 °C
  • Specific Heat Capacity
  • 0.451 J/g-°C @Temperature 500 °C
  • Specific Heat Capacity
  • 0.470 J/g-°C @Temperature 600 °C
  • Specific Heat Capacity
  • 0.595 J/g-°C @Temperature 700 °C
  • Specific Heat Capacity
  • 0.605 J/g-°C @Temperature 800 °C
  • Specific Heat Capacity
  • 0.610 J/g-°C @Temperature 900 °C
  • Specific Heat Capacity
  • 0.627 J/g-°C @Temperature 1000 °C
  • Thermal Conductivity
  • 11.3 W/m-K
  • Thermal Conductivity
  • 12.6 W/m-K @Temperature 100 °C
  • Thermal Conductivity
  • 14.2 W/m-K @Temperature 200 °C
  • Thermal Conductivity
  • 15.9 W/m-K @Temperature 300 °C
  • Thermal Conductivity
  • 17.5 W/m-K @Temperature 400 °C
  • Thermal Conductivity
  • 19.2 W/m-K @Temperature 500 °C
  • Thermal Conductivity
  • 20.9 W/m-K @Temperature 600 °C
  • Thermal Conductivity
  • 22.5 W/m-K @Temperature 700 °C
  • Thermal Conductivity
  • 24.2 W/m-K @Temperature 800 °C
  • Thermal Conductivity
  • 25.8 W/m-K @Temperature 900 °C
  • Thermal Conductivity
  • 27.5 W/m-K @Temperature 1000 °C

  • Electrical Properties
  • Electrical Resistivity
  • 0.000122 ohm-cm
  • Electrical Resistivity
  • 0.0001234 ohm-cm @Temperature 100 °C
  • Electrical Resistivity
  • 0.0001251 ohm-cm @Temperature 200 °C
  • Electrical Resistivity
  • 0.0001267 ohm-cm @Temperature 300 °C
  • Electrical Resistivity
  • 0.0001276 ohm-cm @Temperature 1000 °C
  • Electrical Resistivity
  • 0.000128 ohm-cm @Temperature 400 °C
  • Electrical Resistivity
  • 0.0001295 ohm-cm @Temperature 500 °C
  • Electrical Resistivity
  • 0.0001298 ohm-cm @Temperature 900 °C
  • Electrical Resistivity
  • 0.0001306 ohm-cm @Temperature 600 °C
  • Electrical Resistivity
  • 0.000132 ohm-cm @Temperature 700 °C
  • Electrical Resistivity
  • 0.0001324 ohm-cm @Temperature 800 °C

Alternative products

ShipsFor-Sale.com is a renowned company specializing in the sale of ships. With years of experience in the maritime industry, they have established themselves as a trusted platform for buyers and sellers worldwide. Offering an extensive range of vessels, including cargo ships, tankers, fishing boats, and luxury yachts, lng tankers for sale listing. Their team of knowledgeable professionals provides expert guidance throughout the buying and selling process, ensuring smooth transactions and customer satisfaction. Whether you are a seasoned ship owner or a first-time buyer, ShipsFor-Sale.com offers a comprehensive selection of vessels and a seamless online experience, making them the go-to destination for ship sales.

Andrey Kutuzov

University of Córdoba (Spain), email: [email protected]

3 prices for Haynes 242® alloy, cold reduced sheet, annealed and aged

Seller from Phoenix – 2021-05-23:

Seller from Phoenix work with company: Solvay, Exxon Chemical, SABIC Innovative Plastics (GE Plastics), ALIMEX GmbH

Price: $1542 per MT

Seller from Guangzhou – 2021-04-01:

Seller from Guangzhou work with company: 3M, Solvay, SABIC Innovative Plastics (GE Plastics), ALIMEX GmbH

Price: $1516 per MT

Seller from Tokyo – 2021-07-04:

Seller from Tokyo work with company: 3M, Solvay, RTP Company, SABIC Innovative Plastics (GE Plastics)

Price: $2470 per MT

Share on Pinterest
Share on LinkedIn
Share on Reddit

Would you like to sell Haynes 242® alloy, cold reduced sheet, annealed and aged?

Plastic warehouse

Find a direct plastic supplier if you're interested in a supplier or Used tire shop in Singapore open-nearme.com